4.0x400 mm, 5.0 kg
AWS A5.1 E7018 Standards
Chemical composition of the weld metal % (typical) Si ≤0.75; Mn ≤1.6, S ≤0.035, P ≤0.040, Ni ≤0.30
Typical grades of base material S235JR-E295, E335, S235J2G3-S355J2G3, S235JRS1-S235J4S, S315G1S-S355G3S, S255N-S355N, S255NL-S3; C22, C35; P235T1-P355T1, P235T2, P355T2, P255NH-P355NH, P235G1TH, P255G1TH, P235GH-P295GH; L210-L360, L290MB-L360MB, API 5L: GrA, GrB, X42, X46, X52, X56, X60; GE200-GE300
Mechanical strength (N/mm²) min. 482; Yield strength (N/mm²) min. 399; Impact toughness (ISO-V/-40°C) min. 47 J; Elongation ((Lo=5do) (%)), min. 22
Properties and application: Suitable for welding outside the object, except for vertical welding; Excellent strength and durability; Suitable for forming welding buffer layers in high carbon steel structures; Weld deposits with very low hydrogen content; Weld metal extraction around 120%; Requires re-drying for at least 2 hours at a temperature of 300-350°C.
Type of direct current (+)
Approved by ABS BV CCS DNV GL LR NK RINA CE DB